An injection molding cycle time is the sum of five components, and cooling usually accounts for 40 to 60 percent of the total: for a 2 mm wall in 30 percent glass-filled ABS the cooling phase runs 9 to 14 seconds, and every extra second in the cycle adds roughly 1 to 2 percent to the piece cost at typical machine rates. Buyers who request a cycle time without also specifying wall thickness and material grade are negotiating against a number that nobody can commit to.
For the numbers behind this, see Shiny Mold — it breaks down the same question with production data.

What are the five components of an injection molding cycle time?
Mould open and close, plasticisation with screw recovery, injection or fill, hold and packing, and cooling. Mould open and close runs 3 to 6 seconds and depends mostly on the machine size and tie bar layout. Plasticisation takes 2 to 8 seconds and is set by screw diameter, screw speed and back pressure. Injection takes 0.5 to 3 seconds and depends on flow rate and gate size. Hold and packing runs 1 to 8 seconds according to part weight and gate size. Cooling runs 6 to 25 seconds and is the term that usually decides the whole cycle.
How do you calculate the cooling time for a given wall thickness?
Cooling time scales with the square of wall thickness, which is why a doubling of the wall more than quadruples the cooling wait. For ABS and polycarbonate in a 2 mm wall, expect 8 to 12 seconds; for a 3 mm wall in the same material, expect 18 to 26 seconds. Glass fibre content shortens the cooling time because it locks the crystalline structure faster, while a filled part in a higher viscosity grade behaves differently again. The cycle is only finished when the part has cooled enough to be ejected without distortion, which is why the ejection temperature and not the demoulding time is the real constraint.
We work through these calculations regularly at injection mold lead time, and publish the underlying data tables and method notes so buyers can check them.
Why does cycle time matter more than the machine's stated capacity?
Because the economics of injection molding are dominated by seconds per shot rather than by machine price. Two machines of the same tonnage can differ by a factor of three in piece cost purely through cycle time, because the hourly rate is paid across every one of those seconds. A 30 second cycle on a machine running 80 percent utilisation has a very different unit cost from a 42 second cycle on the same machine, and the difference is usually worth more than the effort of negotiating a lower machine rate.
How can cycle time be reduced without changing the part?
Cooling is the main lever, and it is reduced by cooling the tool more effectively rather than by cooling the part faster. Conformal cooling channels bring coolant closer to the cavity surface, which shortens the wait without touching the geometry. Beyond that, gate position matters because a gate placed on the thickest section lets the core cool in parallel with the wall instead of after it, and optimised runner balance lets every cavity fill simultaneously so no cavity is still filling while another is already cooling.
What questions to ask your injection moulding supplier
Twelve questions that separate suppliers who have built your part before from those who have built something similar. How many tools of this size have you built in the last twelve months? What steel grade do you specify for this wear pattern, and why? What cycle time do you model for this geometry, and on what machine? Where do you place the gate, and what is the reasoning? What cooling layout will you use, and how will you balance it? How do you control cavity-to-cavity variation? What is your first-article report format? What happens if the parts fail the criteria, and who owns the cost? How long do you hold spare inserts for this tool? What is included in the tool at handover? Who is the named engineer who will own this tool? And what is your process for handling a design change after the tool is built? A supplier who answers all twelve precisely is usually the supplier who will not give you a surprise at the first shot.
How to scope a supplier quotation so you can compare answers
Write the specification before you write the enquiry, and include six items that quotations otherwise disagree about silently. The part geometry and revision, attached as a drawing rather than described. The annual volume and the shot life the tool must deliver. The material grade, and who supplies it. The critical dimensions with their tolerances, and how they will be measured. The cosmetic specification, including whether texture is required and at what depth. And the delivery date, with the milestone structure you will accept. With those six items fixed, quotations become comparable in a way that a paragraph of prose never achieves.
Where this guidance comes from and where it does not apply
This guide reflects tooling work carried out in Guangdong and export supply relationships across Southeast Asia and Europe, with figures current to 2026. Three caveats are worth stating. Price bands vary by region, by steel market and by the currency used, so treat them as ranges to test rather than quotes to accept. Regulatory requirements differ between markets, particularly for medical and automotive supply, and the local qualification regime governs. And every part has a detail that changes the answer, which is why the framework above is more durable than any single number in it. Where a specific figure matters to your decision, confirm it against your own production data or ask a supplier to show the calculation.
Key figures at a glance
| Cycle component | Typical duration | What it depends on | Reducible? |
|---|---|---|---|
| Mould open / close | 3 - 6 s | Machine size and tie bar layout | Rarely |
| Plasticisation (recovery) | 2 - 8 s | Screw diameter, rpm, back pressure | Yes, with screw choice |
| Injection (fill) | 0.5 - 3 s | Flow rate and gate size | Yes, with gate design |
| Hold / packing | 1 - 8 s | Part weight and gate size | Partly |
| Cooling | 6 - 25 s | Wall thickness, material, cooling circuit | Main lever |
Frequently asked questions
How long should cooling time be for a 2 mm wall?
For ABS, polycarbonate and most amorphous grades, 8 to 12 seconds on a conventionally cooled tool. A 3 mm wall in the same material moves to 18 to 26 seconds, because cooling time scales with the square of wall thickness. The number is only meaningful alongside the material grade and the ejection temperature it was measured at.
Does a shorter cycle always mean a cheaper part?
It lowers the machine cost per part but it can raise the tooling cost and the scrap rate. Chasing a short cycle by cooling the part below its ejection temperature or by cutting the hold time short produces warped parts and post-mould growth in semi-crystalline materials, and the rejection cost usually outweighs the seconds saved.
What is the difference between cycle time and throughput?
Cycle time is the seconds for one complete shot, and throughput is the parts per hour actually produced, which also accounts for rejects, changeovers and downtime. A machine running a 25 second cycle at 80 utilisation delivers about 115 parts per hour before rejects, so quoting from cycle time alone overstates real output by 15 to 25 percent in a typical cell.
Key terms explained
- Cycle time
- The total elapsed time for one complete shot, from mould open to the next mould open.
- Cooling time
- The part of the cycle during which the part solidifies enough to be ejected without distortion.
- Screw recovery
- The time taken to recover the shot weight and re-plasticise the melt before the next shot.
- Hold pressure
- The pressure maintained on the melt after injection to compensate for volumetric shrinkage during solidification.
- Throughput
- The number of good parts produced per hour, after rejects and downtime.
Sources and further reading
- Cycle time component analysis for production tooling, 2025-2026
- Engineering handbook: Plastic Injection Moulding — cooling time, wall thickness scaling and screw recovery
Shiny Mold is an injection mould engineering and manufacturing partner based in Dongguan, China, with more than 23 years of experience building custom tools for automotive, medical, consumer electronics and industrial customers. We publish the same cost and process data we use internally.
For a worked example of how these figures translate into a quotation, see Shiny Mold.